Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SEETEC VE700 - EVAC - Lotte Chemical Corporation

Material Data Center offers the following functions for SEETEC VE700:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Seetec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 15 g/10min ASTM D 1238
Mechanical propertiesValueUnitTest Standard
ASTM Data
Shore D Hardness 25 - ASTM D 2240
Thermal propertiesValueUnitTest Standard
ASTM Data
Melting Temperature 69 °C ASTM D 3418
Vicat Temperature 40 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 950 kg/m³ ASTM D 792
Characteristics
Features
Good Adhesion, Copolymer
Chemical Resistance
Oxidation Resistance
Applications
Encapsulation
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.