Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Silopren® LSR 2660 - VMQ - Momentive Performance Materials Inc.

Material Data Center offers the following functions for Silopren® LSR 2660:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Silopren datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Appearance/Color:
liquid, transparent

Conformity:
The product meets the requirements for passing the test standards USP Class VI, FDA 21 CFR 177.2600 and ISO 10993.
Based on listing of ingredients in the BfR recommendation XV "Silicones", the product is compositionally compliant.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 9 MPa ISO 37
Strain at break 400 % ISO 37
Shore A hardness 62 - ISO 7619-1
ASTM Data
Tear Strength 45 kN/m ASTM D 624
Thermal propertiesValueUnitTest Standard
ISO Data
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Yellow Card available yes - -
Other propertiesValueUnitTest Standard
Density 1130 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Special Characteristics
Transparent
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR, Drinking water contact, Drinking water contact KTW, Drinking water contact DVGW W270, US Pharmacopeia Class VI Approved
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.