Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SINKRAL® B4 Milano - ABS - Versalis S.p.A

Material Data Center offers the following functions for SINKRAL® B4 Milano:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Sinkral datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Symbol according to ISO 1043-1: ABS

Designation: Thermoplastics ISO 2580-ABS 1,EGN,105-04-16-20

Sinkral B 4 Milano is a special grade for extrusion/thermoforming.
Thanks to its low gel content toghether an optimum balance of stiffness and impact resistance, ensures high aesthetic quality of surfaces, partcularly suitable for co-extrusion.
Optimal thermal stability and rheological properties also permit the sheet production of large dimensions.


Applications:

Exstruded and co-exstruded sheets, including thick sheet where high hot draw ratios are required.
Its excellent surface appearance permit the use in a wide range of applications such as furniture, refrigerator, sanitary, automotive and packaging for foodstuff and industrial items.
Also ideal for the extrusion of profiles for furniture industry.

 

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Density of melt 960 kg/m³ -
Spec. heat capacity of melt 2150 J/(kg K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2300 MPa ISO 527
Yield stress 45 MPa ISO 527
Yield strain 3 % ISO 527
Nominal strain at break 30 % ISO 527
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 140 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 18 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 8 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 109 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 83 °C ISO 75-1/-2
Vicat softening temperature, B 104 °C ISO 306
Coeff. of linear therm. expansion, parallel 90 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.1 - IEC 62631-2-1
Dissipation factor, 1MHz 150 E-4 IEC 62631-2-1
Volume resistivity 1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E14 Ohm IEC 62631-3-2
Electric strength 30 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.6 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1040 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Processing conditions acc. ISO 2580 - ISO ....-2
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Diagrams
Viscosity-shear rate , SINKRAL® B4 Milano, ABS, Versalis
Shearstress-shear rate , SINKRAL® B4 Milano, ABS, Versalis
Dynamic Shear modulus-temperature , SINKRAL® B4 Milano, ABS, Versalis
Stress-strain , SINKRAL® B4 Milano, ABS, Versalis
Secant modulus-strain , SINKRAL® B4 Milano, ABS, Versalis
Specific volume-temperature (pvT) , SINKRAL® B4 Milano, ABS, Versalis
Spec. enthalpy/mass-temp. (DSC) , SINKRAL® B4 Milano, ABS, Versalis
Characteristics
Processing
Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion, Blow Molding, Thermoforming
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Film extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

  Typical processing temperature range:

    Melt temperature           190 - 230 °C

Other extrusion
Other  extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Profile extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Sheet extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com