Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SKYPEL LX780A - TPE - SK Chemicals

Material Data Center offers the following functions for SKYPEL LX780A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Skypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 25 g/10min ASTM D 1238
Temperature 220 °C -
Load 2.16 kg -
Mold Shrinkage, MD 0.007 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Break 27.5 MPa ASTM D 638
Elongation at Break 1500 % ASTM D 638
Modulus at 100% Elongation 3.4 MPa ASTM D 412
Shore A Hardness 80 - ASTM D 2240
Tear Strength 84 kN/m ASTM D 624
Compression Set , 22 hr @ 158 °F 57 % ASTM D 395
Thermal propertiesValueUnitTest Standard
ASTM Data
Melting Temperature 192 °C ASTM D 3418
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.9 % ASTM D 570
Density 1060 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 35 °C -
Zone 1 205 °C -
Zone 2 210 °C -
Zone 3 215 °C -
Nozzle temperature 220 °C -
Processing Recommendation ExtrusionValueUnitTest Standard
Melt temperature 215 °C -
Zone 1 195 °C -
Zone 2 210 °C -
Zone 3 210 °C -
Nozzle temperature 210 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com