Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SKYPEL P147DF - TPE - SK Chemicals

Material Data Center offers the following functions for SKYPEL P147DF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Skypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 18 g/10min ASTM D 1238
Temperature 230 °C -
Load 2.16 kg -
Mold Shrinkage, MD 0.016 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Break 20.6 MPa ASTM D 638
Elongation at Break 400 % ASTM D 638
Flexural Modulus 103 MPa ASTM D 790
Shore D Hardness 47 - ASTM D 2240
Tear Strength 90 kN/m ASTM D 624
Izod Impact notched, 1/4 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 85 °C ASTM D 648
Melting Temperature 216 °C ASTM D 3418
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 1.4 % ASTM D 570
Density 1180 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 40 °C -
Zone 1 220 °C -
Zone 2 230 °C -
Zone 3 230 °C -
Nozzle temperature 235 °C -
Processing Recommendation ExtrusionValueUnitTest Standard
Melt temperature 225 °C -
Zone 1 205 °C -
Zone 2 220 °C -
Zone 3 220 °C -
Nozzle temperature 220 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com