Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Softflex® 0615 - TPE - LyondellBasell Industries

Material Data Center offers the following functions for Softflex® 0615:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Softflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 8.3 g/10min ASTM D 1238
Temperature 235 °C -
Load 1 kg -
Mold Shrinkage, MD 0.011 mm/mm ASTM D 955
Mold Shrinkage, TD 0.011 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 7.79 MPa ASTM D 638
Elongation at Break 750 % ASTM D 638
Flexural Modulus 14.96 MPa ASTM D 790
Modulus at 100% Elongation 1.79 MPa ASTM D 412
Modulus at 300% Elongation 4.48 MPa ASTM D 412
Shore A Hardness 53 - ASTM D 2240
Tear Strength 28.4 kN/m ASTM D 624
Taber Abrasion Resistance 0.192 mg/1000 cycles ASTM D 1044
Gardner Impact 36.2 J ASTM D 2794,4226,5420
Compression Set , 22 hr @ 73 °F 18.4 % ASTM D 395
Other propertiesValueUnitTest Standard
Density 994 kg/m³ ASTM D 792
Characteristics
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.