Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Spectar™ - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Spectar™:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Spectar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Spectar™ Clear is a copolyester, developed by Eastman to achieve measurably improved sheet clarity and edge color while maintaining the performance characteristics for which Eastman Spectar™ copolyester has become known in the industry. It offers the thermoformability and ease of fabrication of Eastman Spectar™ copolyester along with significantly improved clarity. Eastman Spectar™ Clear also offers approximately double the notch impact strength, 50% higher instrumented impact strength and better chemical resistance when compared

to traditional Spectar™ Copolyester.




Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1800 MPa ASTM D 638
Tensile Strength at Yield 48 MPa ASTM D 638
Tensile Strength at Break 53 MPa ASTM D 638
Elongation at Yield 5 % ASTM D 638
Elongation at Break 340 % ASTM D 638
Flexural Modulus 2000 MPa ASTM D 790
Rockwell Hardness R 107 - ASTM D 785
Izod Impact notched, 1/8 in N J/m ASTM D 256
Izod Impact notched, Low-Temperature 83 J/m ASTM D 256
Temperature -30 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating HB - UL 94
Coefficient of Thermal Expansion, MD 76.2 E-6/K ASTM D 696
DTUL @ 66 psi 77 °C ASTM D 648
DTUL @ 264 psi 73 °C ASTM D 648
Vicat Temperature 86 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ASTM Data
Surface Resistivity 1E17 Ohm ASTM D 257
Volume Resistivity 1E16 Ohm*cm ASTM D 257
Arc Resistance 130 s ASTM D 495
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 150 - ASTM D 2457
Haze 0.5 % ASTM D 1003
Light Transmittance 91 % ASTM D 1003
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.19 % ASTM D 570
Density 1230 kg/m³ ASTM D 792
Characteristics
Processing
Sheet Extrusion, Thermoforming
Special Characteristics
High impact or impact modified, Transparent
Features
Low Odor, Copolymer
Chemical Resistance
General Chemical Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.