Supol - PP - LyondellBasell Industries
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Supol" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
Supol HG960E | PP-GX30 |
Supol HP1700E | PP |
Supol HP190E | PP |
Supol HP310E | PP |
Supol HP908E | PP |
Supol HP908UE BLACK | PP |
Supol HR525E | PP-MX |
Supol HR570E | PP-MX |
Supol HR570E BLACK | PP-MX |
Supol HR570UE | PP-MX |
Supol HR580 | PP-MX |
Supol HR920E | PP-MX |
Supol HR980E | PP-MX |
Supol HR980UE | PP-MX |
Supol HT121E | PP-X |
Supol HT125E | PP-X |
Supol HT143E | PP-MX |
Supol HT144HE | PP-MX |
Supol HT145E | PP-X |
Supol HT240E | PP-MX |
Supol HT245E | PP-MX |
Supol HT310E | PP-MX |
Supol HT315E | PP-X |
Supol HT320E | PP-MX |
Supol HT340E | PP-MX |
Supol HT345E | PP-X |
Supol HT940UE | PP-MX |
Supol HT950E | PP-MX |
Supol HT960E BLACK | PP-MX30 |
Supol HT980UE BLACK | PP-MX40 |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.