Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SUPRAN® PP1350 - PP-GF50 - Lotte Chemical Corporation

Material Data Center offers the following functions for SUPRAN® PP1350:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Supran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.002 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength 140 MPa ASTM D 638
Flexural Modulus 9800 MPa ASTM D 790
Flexural Strength 186 MPa ASTM D 790
Rockwell Hardness R 110 - ASTM D 785
Izod Impact notched, 1/8 in 294 J/m ASTM D 256
Izod Impact notched, Low-Temperature 304 J/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 264 psi 165 °C ASTM D 648
Other propertiesValueUnitTest Standard
Density 1310 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 40 - 70 °C -
Zone 1 215 - 230 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
High impact or impact modified
Features
Creep Resistance, Long fiber reinforced, Low Warpage
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.