Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TENAC™ 4013A - POM - Asahi Kasei

Material Data Center offers the following functions for TENAC™ 4013A:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tenac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 8.6 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Melt flow index, MFI 10 g/10min ISO 1133
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3000 MPa ISO 527
Yield stress 70 MPa ISO 527
Strain at break 40 % ISO 527
Flexural modulus, 23°C 2700 MPa ISO 178
Charpy notched impact strength, +23°C 10 kJ/m² ISO 179/1eA
ASTM Data
Tensile Strength 67 MPa ASTM D 638
Elongation at Break 45 % ASTM D 638
Flexural Modulus 2900 MPa ASTM D 790
Flexural Strength 98 MPa ASTM D 790
Rockwell Hardness M 94 - ASTM D 785
Taber Abrasion Resistance 13 mg/1000 cycles ASTM D 1044
Izod Impact notched, 1/8 in 85 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 102 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 164 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 100 E-6/K ISO 11359-1/-2
ASTM Data
Coefficient of Thermal Expansion, MD 100 E-6/K ASTM D 696
DTUL @ 66 psi 172 °C ASTM D 648
DTUL @ 264 psi 136 °C ASTM D 648
Electrical propertiesValueUnitTest Standard
ASTM Data
Dielectric Strength, Short Time 18 kV/mm ASTM D 149
Surface Resistivity 1E17 Ohm ASTM D 257
Volume Resistivity 1E16 Ohm*cm ASTM D 257
Arc Resistance 250 s ASTM D 495
Other propertiesValueUnitTest Standard
Density 1420 kg/m³ ISO 1183
Water Absorption, 24hr 0.2 % ASTM D 570
Density 1420 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 - 4 h -
Melt temperature 190 - 210 °C -
Mold temperature 60 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets
Special Characteristics
U.V. stabilized or stable to weather
Features
Homopolymer
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com