Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ LX150HF - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ LX150HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Tritan™ LX150HF copolyester is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan™ LX150HF has viscosity reductions of 40-50% relative to standard grades of Eastman Tritan™. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and

chemical resistance. Tritan™ LX150HF was developed for the cosmetic, fragrance, and personal care markets.

Tritan™ LX150HF can easily be converted into articles for application in consumer and personal care markets by injection molding, extrusion blow molding, and injection blow molding.

Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1575 MPa ASTM D 638
Tensile Strength at Yield 43 MPa ASTM D 638
Tensile Strength at Break 52 MPa ASTM D 638
Elongation at Yield 7 % ASTM D 638
Elongation at Break 210 % ASTM D 638
Flexural Modulus 1575 MPa ASTM D 790
Rockwell Hardness R 111 - ASTM D 785
Izod Impact notched, 1/8 in 860 J/m ASTM D 256
Izod Impact notched, Low-Temperature 110 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 81 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 91 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1180 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 88 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 260 - 282 °C -
Mold temperature 38 - 66 °C -
Characteristics
Processing
Injection Molding, Blow Molding
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat, Transparent
Features
Amorphous, Copolymer
Chemical Resistance
General Chemical Resistance, Hydrolytically Stable
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.