Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TYRIL™ 867 E UV - SAN - Trinseo

Material Data Center offers the following functions for TYRIL™ 867 E UV:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tyril datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 4 g/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
ASTM Data
Melt Flow Index, MFI 4 g/10min ASTM D 1238
Temperature 230 °C -
Load 3.8 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3700 MPa ISO 527
Stress at break 70 MPa ISO 527
Charpy impact strength, +23°C 17 kJ/m² ISO 179/1eU
Izod impact strength, +23°C 14 kJ/m² ISO 180/1U
Rockwell hardness M83 - ISO 2039-2
ASTM Data
Tensile Modulus 3702 MPa ASTM D 638
Tensile Strength at Break 70.3 MPa ASTM D 638
Flexural Strength 97.2 MPa ASTM D 790
Rockwell Hardness M 83 - ASTM D 785
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, A 110 °C ISO 306
Vicat softening temperature, B 101 °C ISO 306
Coeff. of linear therm. expansion, parallel 50 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm -
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 1.6 mm -
Vicat Temperature 101 °C ASTM D 1525
Specific Heat 878 J/(kg K) ASTM C 351
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Dissipation factor, 1MHz 1 E-4 IEC 62631-2-1
Electric strength 9.1 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Density 1080 kg/m³ ISO 1183
Density 1080 kg/m³ ASTM D 792
Characteristics
Processing
Sheet Extrusion, Thermoforming
Special Characteristics
U.V. stabilized or stable to weather, Heat stabilized or stable to heat, Transparent
Chemical Resistance
General Chemical Resistance
Regional Availability
Europe, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.