Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 1520 FC R01 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 1520 FC R01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Ultradur® B1520 FC R01 UN is suitable for plastic parts, where material approval regarding direct food contact is a mandatory requirement.

The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including European Food Contact (EU) Nr. 10/2011 and GMP (EC) N°2023/2006.

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).

The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 100 cm³/10min ISO 1133
Temperature 250 °C -
Load 2.16 kg -
Molding shrinkage, parallel 1.9 % ISO 294-4, 2577
Molding shrinkage, normal 1.8 % ISO 294-4, 2577
Ejection temperature 160 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2500 MPa ISO 527
Yield stress 58 MPa ISO 527
Yield strain 4 % ISO 527
Nominal strain at break 12 % ISO 527
Charpy impact strength, +23°C 130 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 40 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 3 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 2.5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 223 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 55 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 150 °C ISO 75-1/-2
Vicat softening temperature, B 180 °C ISO 306
Coeff. of linear therm. expansion, parallel 115 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 115 E-6/K ISO 11359-1/-2
Other propertiesValueUnitTest Standard
Water absorption 0.5 % Sim. to ISO 62
Humidity absorption 0.25 % Sim. to ISO 62
Density 1310 kg/m³ ISO 1183
Material specific propertiesValueUnitTest Standard
ISO Data
Viscosity number 88 cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 260 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 120 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.04 % -
Melt temperature 260 - 280 °C -
Mold temperature 20 - 60 °C -
Diagrams
Viscosity-shear rate , Ultradur® B 1520 FC R01, PBT, BASF
Shearstress-shear rate , Ultradur® B 1520 FC R01, PBT, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Certifications
Food contact, Food approval 10/2011
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 260 - 280 °C
injection molding, Melt temperature, recommended: 275 °C
injection molding, Mold temperature, range: 20 - 60 °C
injection molding, Mold temperature, recommended: 40 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com