Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4040 G4 - (PBT+PET)-GF20 - BASF

Material Data Center offers the following functions for Ultradur® B 4040 G4:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Injection moulding grade with 20 % glass fibres for technical parts, with excellent surface quality for oven door handles, car door handles.

Abbreviated designation according to ISO 1043: PBT-PET-GF20
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 22 cm³/10min ISO 1133
Temperature 275 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.4 % ISO 294-4, 2577
Molding shrinkage, normal 0.9 % ISO 294-4, 2577
Density of melt 1240 kg/m³ -
Thermal conductivity of melt 0.175 W/(m K) -
Spec. heat capacity of melt 1880 J/(kg K) -
Ejection temperature 170 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 7500 MPa ISO 527
Stress at break 120 MPa ISO 527
Strain at break 2.8 % ISO 527
Charpy impact strength, +23°C 40 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 40 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 5.5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 223 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 180 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 215 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 35 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 105 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.7 - IEC 62631-2-1
Relative permittivity, 1MHz 3.5 - IEC 62631-2-1
Dissipation factor, 100Hz 14 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 180 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E13 Ohm IEC 62631-3-2
Electric strength 36 kV/mm IEC 60243-1
Comparative tracking index 300 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1470 kg/m³ ISO 1183
Material specific propertiesValueUnitTest Standard
ISO Data
Viscosity number 105 cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 270 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 120 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.04 % -
Melt temperature 250 - 280 °C -
Mold temperature 60 - 100 °C -
Diagrams
Viscosity-shear rate , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Shearstress-shear rate , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Dynamic Shear modulus-temperature , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Stress-strain , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Secant modulus-strain , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Specific volume-temperature (pvT) , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Tensile modulus-temperature , Ultradur® B 4040 G4, (PBT+PET)-GF20, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 280 °C
injection molding, Melt temperature, recommended: 270 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 80 °C
Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Application examples
Housing, light switch
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.