Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse BVOH - PVAL - BASF

Material Data Center offers the following functions for Ultrafuse BVOH:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 11.4 cm³/10min ISO 1133
Temperature 210 °C -
Load 2.16 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 175 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 69 °C ISO 11357-1/-2
Other propertiesValueUnitTest Standard
Density 1140 kg/m³ ISO 1183
3D DataValueUnitTest Standard
Other Standards[S]
Tensile modulus, flat 2340 MPa ISO 527
Tensile modulus, upright 1430 MPa ISO 527
Tensile strength, flat 33.7 MPa ISO 527
Tensile strength, upright 8.7 MPa ISO 527
Strain at break, flat 14.8 % ISO 527
Strain at break, upright 0.6 % ISO 527
Flexural modulus, flat 2240 MPa ISO 178
Flexural modulus, on-edge 1810 MPa ISO 178
Flexural modulus, upright 1080 MPa ISO 178
Flexural strength, flat 53.8 MPa ISO 178
Flexural strength, on-edge 50.3 MPa ISO 178
Flexural strength, upright 11.4 MPa ISO 178
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.