Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Ultramid A - PA66 - BASF

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Ultramid A" in Material Data Center leads to the following information:

Tradename: Ultramid A
Family: PA66
Producer: BASF
93 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Ultramid® A27 E PA66
Ultramid® A34 01 PA66
Ultramid® A3EG10 PA66-GF50
Ultramid® A3EG3 PA66-GF15
Ultramid® A3EG5 PA66-GF25
Ultramid® A3EG6 PA66-GF30
Ultramid® A3EG6 BK00564 PA66
Ultramid® A3EG7 PA66-GF35
Ultramid® A3EG7 EQ BK23189 PA66-GF35
Ultramid® A3EG7 FC Aqua UN PA66-GF35
Ultramid® A3HG2 PA66-GF10
Ultramid® A3HG5 PA66-GF25
Ultramid® A3HG6 HR BK23591 PA66-GF30
Ultramid® A3HG6 WIT BK20560 (PA66+PA6T/6)-(GF+GB)30
Ultramid® A3HG7 PA66-GF35
Ultramid® A3K FC Aqua UN PA66
Ultramid® A3L HP PA66
Ultramid® A3SK PA66
Ultramid® A3UG5 PA66-GF25 FR(40+30)
Ultramid® A3W PA66
Ultramid® A3W R01 SW805 PA66
Ultramid® A3W2G10 BK20560 PA66-GF50
Ultramid® A3WC4 PA66-CF20
Ultramid® A3WG10 PA66-GF50
Ultramid® A3WG3 PA66-GF15
Ultramid® A3WG5 PA66-GF25
Ultramid® A3WG6 PA66-GF30
Ultramid® A3WG6 HRX BK23591 PA66-GF30
Ultramid® A3WG7 PA66-GF35
Ultramid® A3WG7 HP BK20560 PA66-GF35
Ultramid® A3WG8 BK20560 PA66-GF40
Ultramid® A3WGM53 BK20560 PA66-(GF+MD)40
Ultramid® A3X2G10 PA66-GF50 FR(52)
Ultramid® A3X2G5 PA66-GF25 FR(52)
Ultramid® A3X2G7 PA66-GF35 FR(52)
Ultramid® A3X3G5 PA66-GF25
Ultramid® A3X3G7 PA66-GF35
Ultramid® A3XZG5 PA66-I-GF25 FR(52)
Ultramid® A3Z PA66-I
Ultramid® A3Z HP PA66-I
Ultramid® A3Z3 PA66
Ultramid® A3ZG3 HP BK20465 PA66-GF15
Ultramid® A3ZG6 BK20591 PA66-I-GF30
Ultramid® A4H PA66
Ultramid® A3W2G6 BK20560 (PA66+PA6)-GF30
Ultramid® A3L HP BK20465 PA66
Ultramid® A3Z HP BK20465 PA66
Ultramid® A3ZG7 OSI BK23273 PA66-I-GF35
Ultramid® A3U42G6 (PA66+PA6)-GF30 FR(40)
Ultramid® A3K R01 PA66
Ultramid® A3W2G7 BK20560 (PA66+PA6)-GF35
Ultramid® A3WC8 PA66-CF40
Ultramid® A3WG7 HRX BK23591 PA66-GF35
Ultramid® Advanced N3HG6 UN PA9T-GF30
Ultramid® Advanced N4H UN PA9T
Ultramid® Advanced N3HG6 LS BK PA9T-GF30
Ultramid® Advanced N3WG6 LS BK PA9T-GF30
Ultramid® Advanced N4WG7 LS BK PA9T-GF35
Ultramid® A3EG6 FC PA66-GF30
Ultramid® A3WG10 HP BK23325 PA66-GF50
Ultramid® A3WG7 OSI BK20560 PA66-GF35
Ultramid® A3WG6 LT BK PA66-GF30
Ultramid® Advanced N3U41G6 PA9T-GF30 FR(40)
Ultramid® Advanced N4U41 LS BK PA9T FR(40)
Ultramid® Advanced T2340G6 PA6T/66-GF30 FR(40)
Ultramid® Advanced N2U40G7 LS BK23300 PPA-GF35
Ultramid® Advanced N2U40G7 UN PA9T FR
Ultramid® Advanced N2U40G7 LS BK PA9T-GF35 FR
Ultramid® Advanced N3HG6 LT BK PA9T-GF30
Ultramid® Advanced N4HG7 LS BK23593 PA9T-GF35
Ultramid® A4H R01 PA66
Ultramid® A3XZC3 ESD bk 23187 PA66-CF15
Ultramid® Advanced N3U40G6 PPA-GF30
Ultramid® Advanced T2300HG6 LS sw23346 PA6T/66-GF30
Ultramid® A3EG10 FC Aqua BK23285 PA66-GF50
Ultramid® A3EG10 HP PA66-GF50
Ultramid® A3EG7 FC Aqua BK23285 PA66-GF35
Ultramid® A3K FC R01 PA66
Ultramid® A3K R02 BK00464 PA66
Ultramid® A3L HP UV BK23220 PA66
Ultramid® A3WG4 PA66-GF20
Ultramid® A3WG10 CR bk564 PA66-GF50
Ultramid® A3X2G5 R02 PA66-GF25 FR(52)
Ultramid® A3X2G7 R02 PA66-GF35 FR
Ultramid® Advanced T1000HG10 LS BK PA6T/6I-GF50
Ultramid® Advanced T1000HG6 LS BK PA6T/6I-GF30
Ultramid® Advanced T1000HG6 un PA6T/6I-GF30
Ultramid® Advanced T1000HG7 LS BK23593 PA6T/6I-GF35
Ultramid® Advanced T1000HG7 un PA6T/6I-GF35
Ultramid® A3HG6 HR PA66-GF30
Ultramid® A3Z HP UV PA66
Ultramid® Advanced N2U40G5 LS BK23389 PA9T-GF25 FR
Ultramid® A3WG7 CR bk564 PA66-GF35

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.