Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 black CF - PA11-CF - BASF

Material Data Center offers the following functions for Ultrasint PA11 black CF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 9 / * cm³/10min ISO 1133
Temperature 220 / * °C -
Load 2.16 / * kg -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 202 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 151 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 189 / * °C ISO 75-1/-2
Vicat softening temperature, A 193 / * °C ISO 306
Vicat softening temperature, B 188 / * °C ISO 306
Other propertiesdry / condUnitTest Standard
Density 1070 / - kg/m³ ISO 1183
Bulk density 540 kg/m³ -
3D Datadry / condUnitTest Standard
Other Standards[S]
Tensile modulus, flat 5900 / 4550 MPa ISO 527
Tensile modulus, upright 2500 / 2000 MPa ISO 527
Tensile strength, flat 82 / 71 MPa ISO 527
Tensile strength, upright 55 / 48 MPa ISO 527
Strain at break, flat 7 / 11 % ISO 527
Strain at break, upright 11 / 17 % ISO 527
Flexural modulus, flat 5800 / 5000 MPa ISO 178
Flexural modulus, upright 2500 / 2100 MPa ISO 178
Charpy impact strength, +23°C, flat 54 / 63 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 33 / 51 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 6.4 / 6.7 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 4.7 / 4.7 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, flat 48 / 52 kJ/m² ISO 180/1U
Izod impact strength, +23°C, upright 34 / 45 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, flat 8.7 / 8.5 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, upright 5 / 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing, Laser Sintering
Delivery form
Powder, Black
Special Characteristics
Increased electrical conductivity, High impact or impact modified
Chemical Resistance
General Chemical Resistance, Oil Resistance
Certifications
Contains renewable resources
Applications
Automotive, Electrical and Electronical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.