Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA6 FR black - PA6 - BASF

Material Data Center offers the following functions for Ultrasint PA6 FR black:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 10 / * cm³/10min ISO 1133
Temperature 240 / * °C -
Load 2.16 / * kg -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 218 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 113 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 207 / * °C ISO 75-1/-2
Vicat softening temperature, A 214 / * °C ISO 306
Vicat softening temperature, B 197 / * °C ISO 306
Burning behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 750 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.6 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Other propertiesdry / condUnitTest Standard
Density 1300 / - kg/m³ ISO 1183
Bulk density 550 kg/m³ -
3D Datadry / condUnitTest Standard
Other Standards[S]
Tensile modulus, flat 4750 / 2450 MPa ISO 527
Tensile modulus, upright 4500 / 2450 MPa ISO 527
Tensile strength, flat 56 / 41 MPa ISO 527
Tensile strength, upright 33 / 27 MPa ISO 527
Strain at break, flat 1.4 / 2.6 % ISO 527
Strain at break, upright 0.8 / 1.2 % ISO 527
Flexural modulus, flat 4400 / 2000 MPa ISO 178
Flexural modulus, upright 3850 / 2050 MPa ISO 178
Charpy impact strength, +23°C, flat 4.8 / 7.4 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 2.5 / 3.6 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 1.3 / 1.6 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 1 / 1.1 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, flat 5 / 7 kJ/m² ISO 180/1U
Izod impact strength, +23°C, upright 3.4 / 3.8 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, flat 1.8 / 2.1 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, upright 1.5 / 1.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing, Laser Sintering
Delivery form
Powder, Black
Special Characteristics
Flame retardant
Features
Thermal Stability
Applications
Aircraft and Aerospace, Automotive, Electrical and Electronical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.