Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VECTRA® B230 - LCP-CF30 - Celanese

Material Data Center offers the following functions for VECTRA® B230:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vectra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Exceptional strength and stiffness. Suitable for metal replacement applications. Electrically conductive. 30% carbon fiber reinforced. Chemical abbreviation according to ISO 1043-1 : LCP Inherently flame retardant UL-Listing V-0 at 0.46mm thickness per UL 94 flame testing. Relative-Temperature-Index (RTI) according to UL 746B: electrical 130°C, mechanical 130°C. UL = Underwriters Laboratories (USA)

Flammability at thickness hV-0-
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, normal 0.1 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 31800 MPa ISO 527
Stress at break 200 MPa ISO 527
Strain at break 0.7 % ISO 527
Charpy impact strength, +23°C 15 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 280 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 235 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 250 °C ISO 75-1/-2
Vicat softening temperature, B 167 °C ISO 306
Coeff. of linear therm. expansion, parallel 1 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 9 E-6/K ISO 11359-1/-2
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 32 - IEC 62631-2-1
Volume resistivity 1000 Ohm*m IEC 62631-3-1
Surface resistivity 100 Ohm IEC 62631-3-2
Other propertiesValueUnitTest Standard
Density 1500 kg/m³ ISO 1183
Diagrams
Stress-strain , VECTRA® B230, LCP-CF30, Celanese
Secant modulus-strain , VECTRA® B230, LCP-CF30, Celanese
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Increased electrical conductivity, Anti-static, Flame retardant, Light stabilized or stable to light
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
Vectra resins are well known for their excellent thermal and hydrolytic stability. In order to ensure these properties are optimum, the resin should be dried correctly prior to processing. Vectra B-grades should be dried at 150 C for a minimum of 6 hours in a desiccant dryer.
A three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flights may be needed for smaller machines: 1/2 feed, 1/4 compression, 1/4 metering.

Vectra LCPs are shear thinning, their melt viscosity decreases quickly as shear rate increases. For parts that are difficult to fill, the molder can increase the injection velocity to improve melt flow.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.