Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VECTRA® MT®1310 - (LCP+PTFE)-GF30 - Celanese

Material Data Center offers the following functions for VECTRA® MT®1310:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vectra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Vectra® MT1310 VF3001 (natural) is a 30% glass reinforced, easy flow LCP grade for injection molding.

Vectra® MT1310 VF3001 (natural) is a special grade developed for medical industry applications and complies with:
  • Food Contact Substance Notification (FCN) No. 742 of the Food and Drug Administration (FDA) and is listed in the Drug Master File (DMF 8464) and the Device Master File (MAF 315)
  • the corresponding EU and national registry regulatory requirements
  • biocompatibility in tests corresponding to USP 23 Class VI/ISO 10993
  • low residual monomers
  • no animal products
The Standard for the Industry. Excellent balance of properties, including easy flow, easy processing, thermal stability, chemical resistance, mechanical and electrical properties. Suitable for vapor phase surface mount electrical and electronic devices. 
Chemical abbreviation according to ISO 1043-1 : LCP
Inherently flame retardant

Flammability at thickness hV-0-
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.2 % ISO 294-4, 2577
Molding shrinkage, normal 0.4 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 15000 MPa ISO 527
Stress at break 190 MPa ISO 527
Strain at break 2.1 % ISO 527
Charpy notched impact strength, +23°C 46 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 280 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 235 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 250 °C ISO 75-1/-2
Vicat softening temperature, B 160 °C ISO 306
Coeff. of linear therm. expansion, parallel 6 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 23 E-6/K ISO 11359-1/-2
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Oxygen index 45 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.2 - IEC 62631-2-1
Relative permittivity, 1MHz 3.7 - IEC 62631-2-1
Dissipation factor, 100Hz 160 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 180 E-4 IEC 62631-2-1
Volume resistivity 1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 31 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Humidity absorption 0.04 % Sim. to ISO 62
Density 1620 kg/m³ ISO 1183
Diagrams
Dynamic Shear modulus-temperature , VECTRA® MT®1310, (LCP+PTFE)-GF30, Celanese
Stress-strain , VECTRA® MT®1310, (LCP+PTFE)-GF30, Celanese
Secant modulus-strain , VECTRA® MT®1310, (LCP+PTFE)-GF30, Celanese
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Natural Color
Special Characteristics
Flame retardant, Light stabilized or stable to light, Sterilizable, Ethylene Oxide (EtO) Sterilization, Steam sterilization, Gamma irradiation sterilization
Features
Thermal Stability
Chemical Resistance
General Chemical Resistance
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR, Food contact notification (FCN), Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved, Drug Master File, Device Master File
Applications
Medical
Regional Availability
North America, Europe
Other text information
Injection molding
Vectra resins are well known for their excellent thermal and hydrolytic stability. In order to ensure these properties are optimum, the resin should be dried correctly prior to processing. The Vectra MT-grades MT1300, MT1305, MT1310, MT1335, MT1340 and MT1345 should be dried at 150°C for a minimum of 4 hours in a desiccant dryer.
A three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flights may be needed for smaller machines: 1/2 feed, 1/4 compression, 1/4 metering.

Vectra LCPs are shear thinning, their melt viscosity decreases quickly as shear rate increases. For parts that are difficult to fill, the molder can increase the injection velocity to improve melt flow.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.