Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 4000 CF20 - PEEK-CF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 4000 CF20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Carbon fiber-reinforced (20%), high viscosity polyether ether ketone

VESTAKEEP® 4000 CF20 is a carbon fiber reinforced (20%) polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CF20 are of low flammability.

VESTAKEEP® 4000 CF20 can be processed by common injection molding machines for thermoplastics.

We recommend a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 4000 CF20 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

For information about processing VESTAKEEP® 4000 CF20, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines.“

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT WWW.INDUSTRIAL.VESTAKEEP.COM
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 42 cm³/10min ISO 1133
Temperature 400 °C -
Load 21.6 kg -
Molding shrinkage, parallel 0.7 % ISO 294-4, 2577
Molding shrinkage, normal 1.0 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 16859 MPa ISO 527
Stress at break 200 MPa ISO 527
Strain at break 2.5 % ISO 527
Other propertiesValueUnitTest Standard
Density 1360 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 420 °C ISO 294
Injection Molding, mold temperature 200 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Features
Thermal Stability
Chemical Resistance
General Chemical Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com