Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® Care M40 R - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® Care M40 R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
High viscosity, unreinforced polyether ether ketone designed for the medical device industry
VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment.

VESTAKEEP® Care M40 R are semi finished goods based on the high viscosity VESTAKEEP® Care M40 G polymer resin. 

The semi-crystalline polymer features superior thermal and chemical resistance.

Biocompatibility of VESTAKEEP® Care
In an extensive testing program run by independent certified labs, biocompatibility has been tested following United States Pharmacopeia and ISO 10933-1:2003 guidelines.
The test reports attest VESTAKEEP® Care’s excellent biocompatibility.

Biocompatibility tests for VESTAKEEP® Care:

 
Delivery of VESTAKEEP® Care
VESTAKEEP® Care M40 R rods can be produced in various diameters ranging from 6 mm up to 100 mm. The standard length is 1 m. Other dimensions are also available upon request.

Mechanical properties are evaluated on stock shapes test bars and further values are evaluated on injection molded samples.
The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 11 cm³/10min ISO 1133
Temperature 380 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 4050 MPa ISO 527
Yield stress 110 MPa ISO 527
Yield strain 5 % ISO 527
Nominal strain at break 40 % ISO 527
Shore D hardness 84 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 155 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 205 °C ISO 75-1/-2
Vicat softening temperature, B 305 °C ISO 306
Coeff. of linear therm. expansion, parallel 60 E-6/K ISO 11359-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 2.8 - IEC 62631-2-1
Other propertiesValueUnitTest Standard
Water absorption 0.5 % Sim. to ISO 62
Density 1300 kg/m³ ISO 1183
Characteristics
Delivery form
Semifinished product
Features
Thermal Stability
Chemical Resistance
General Chemical Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.