Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ML-GB30 - PA12-GB30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ML-GB30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Microglass bead-filled (30%) PA12 resin for the injection moulding of rigid, low-warpage and dimensionally accurate mouldings

 

Biocompatibility of VESTAMID® Care
VESTAMID® Care ML grades were tested on biocompatibility for applications within the body of up to 30 days contact time and comply with USP <88> class VI and ISO 10993 standards.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation
 
Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 



FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY


 

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 100 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.6 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.7 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2100 / 1800 MPa ISO 527
Yield stress 47 / 37 MPa ISO 527
Yield strain 5 / 5 % ISO 527
Nominal strain at break 20 / >50 % ISO 527
Tensile creep modulus, 1h * / 1600 MPa ISO 899-1
Tensile creep modulus, 1000h * / 1100 MPa ISO 899-1
Charpy impact strength, +23°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Charpy impact strength, -30°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Charpy notched impact strength, +23°C 4.4 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Charpy notched impact strength, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 55 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 150 / * °C ISO 75-1/-2
Vicat softening temperature, B 155 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 130 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 130 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.1 / 5 - IEC 62631-2-1
Relative permittivity, 1MHz 3.5 / 4 - IEC 62631-2-1
Dissipation factor, 100Hz 310 / 600 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 230 / 370 E-4 IEC 62631-2-1
Volume resistivity >1E13 / 2E12 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E15 Ohm IEC 62631-3-2
Electric strength - / 36 kV/mm IEC 60243-1
Comparative tracking index 600 / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 0.5 / * % Sim. to ISO 62
Density 1250 / 1260 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
Shearstress-shear rate , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
Dynamic Shear modulus-temperature , VESTAMID® Care ML-GB30 (dry), PA12-GB30, Evonik
Stress-strain , VESTAMID® Care ML-GB30 (dry), PA12-GB30, Evonik
Secant modulus-strain , VESTAMID® Care ML-GB30 (dry), PA12-GB30, Evonik
Stress-strain (isochronous) 23°C, VESTAMID® Care ML-GB30 (cond.), PA12-GB30, Evonik
Creep modulus-time 23°C, VESTAMID® Care ML-GB30 (cond.), PA12-GB30, Evonik
Creep curve 23°C, VESTAMID® Care ML-GB30 (cond.), PA12-GB30, Evonik
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Features
Low Warpage
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.