Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® D22 - PA612 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® D22:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

High-viscosity PA 612 resin

VESTAMID® D22 is a high-viscosity Polyamide 612 compound for extrusion and injection moulding of e.g. films, monofilaments (abrasive bristles).

The material based on  PA612 absorbs only small amounts of water. Components made of this material  therefore show excellent dimensional stability under changing ambient humidity.

VESTAMID® D22 is supplied as cylindrical granules in moisture-proof polyethylene containers ready for processing.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general recommendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 60 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 1.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.7 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2200 / 1700 MPa ISO 527
Yield stress 59 / 49 MPa ISO 527
Yield strain 4 / 20 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Tensile creep modulus, 1h * / 1800 MPa ISO 899-1
Tensile creep modulus, 1000h * / 600 MPa ISO 899-1
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 5 / 10 kJ/m² ISO 179/1eA
Type of failure C / C - -
Charpy notched impact strength, -30°C 7 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 215 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 60 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 140 / * °C ISO 75-1/-2
Vicat softening temperature, B 180 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 130 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 120 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.8 / 5 - IEC 62631-2-1
Relative permittivity, 1MHz 3 / 3.7 - IEC 62631-2-1
Dissipation factor, 100Hz 230 / 650 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 290 / 550 E-4 IEC 62631-2-1
Volume resistivity >1E13 / 3E12 Ohm*m IEC 62631-3-1
Surface resistivity * / >1E15 Ohm IEC 62631-3-2
Electric strength 27 / 27 kV/mm IEC 60243-1
Comparative tracking index 600 / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 2.7 / * % Sim. to ISO 62
Humidity absorption 1 / * % Sim. to ISO 62
Density 1060 / 1060 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 270 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Diagrams
Specific volume-temperature (pvT) , VESTAMID® D22, PA612, Evonik
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion
Delivery form
Pellets
Applications
Monofilament
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.