Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9008 BK 9.7504 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9008 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

High-viscosity, plasticizer-free extrusion compound with an extraordinary long-term heat resistance

VESTAMID® LX9008 BK 9.7504 is a plasticizer-free polyamide 12 compound, with an especially high long-term resistance under thermal load.

VESTAMID®  LX9008 BK 9.7504 is suitable to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel.

The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions.

Using VESTAMID® LX9008 BK 9.7504 for fuel lines one must pay attention to certain preconditions. The Technical Marketing Department gives you advice in selecting the suitable VESTAMID® compound.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.2 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.9 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1450 / 970 MPa ISO 527
Yield stress 41 / 39 MPa ISO 527
Yield strain 5 / 17 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 40 / 90 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 22 / 22 kJ/m² ISO 179/1eA
Type of failure C / C - -
Shore D hardness 73 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 176 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 47 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 48 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 113 / * °C ISO 75-1/-2
Vicat softening temperature, B 145 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 90.5 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 120 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.7 / 4.7 - IEC 62631-2-1
Relative permittivity, 1MHz 2.9 / 3.1 - IEC 62631-2-1
Dissipation factor, 100Hz 520 / 1040 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 320 / 390 E-4 IEC 62631-2-1
Volume resistivity 1E12 / 2.3E10 Ohm*m IEC 62631-3-1
Electric strength 38 / 37 kV/mm IEC 60243-1
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.4 / * % Sim. to ISO 62
Humidity absorption 0.7 / * % Sim. to ISO 62
Density 1010 / - kg/m³ ISO 1183
Characteristics
Processing
Pipe/Tube Extrusion, Profile Extrusion, Other Extrusion
Delivery form
Pellets, Black
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.