Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ML17 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ML17:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Low viscosity polyamide 12 for medical application

VESTAMID® Care ML17 is resistant to body fluids and toxicologically safe.
 

Typical application areas for filled VESTAMID Care ML grades include  catheters, housing parts, monitoring and imaging devices and durable medical equipment.

Advantages at a glance

- High impact resistance

- Easy processability & colorability

- Low sliding friction

- High toughness

- High abrasion resistance

- Density 1.0 g/cc

- High dimensional stability

- High chemical resistance

- Gamma and EtO sterilizable


Biocompatibility of VESTAMID® Care ML
VESTAMID® Care ML grades were tested on biocompatibility for applications within the body of up to 30 days contact time and comply with USP <88> class VI and ISO 10993 standards.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation
Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 21 / * cm³/10min ISO 1133
Temperature 210 / * °C -
Load 2.16 / * kg -
Molding shrinkage, parallel 0.7 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.2 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1400 / 1120 MPa ISO 527
Yield stress 43 / 41 MPa ISO 527
Yield strain 5 / 13 % ISO 527
Nominal strain at break >50 / 40 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / 50 kJ/m² ISO 179/1eU
Type of failure - / C(N) - -
Charpy notched impact strength, +23°C 4.5 / 4.5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Charpy notched impact strength, -30°C 6 / 5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Shore D hardness 75 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 45 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 110 / * °C ISO 75-1/-2
Vicat softening temperature, B 140 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 150 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.8 / - - IEC 62631-2-1
Relative permittivity, 1MHz 2.9 / - - IEC 62631-2-1
Dissipation factor, 100Hz 500 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 281 / - E-4 IEC 62631-2-1
Volume resistivity >1E13 / 2.3E12 Ohm*m IEC 62631-3-1
Other propertiesdry / condUnitTest Standard
Water absorption 1.5 / * % Sim. to ISO 62
Humidity absorption 0.7 / * % Sim. to ISO 62
Density 1020 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
High impact or impact modified, Sterilizable, Ethylene Oxide (EtO) Sterilization, Gamma irradiation sterilization
Features
Tribologic Grade
Chemical Resistance
General Chemical Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com