Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® E62-S3 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® E62-S3:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Heat- and light-stabilized compound based on polyamide 12 elastomer for molding of sport shoe soles

VESTAMID® E62-S3 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer.

The VESTAMID® E represent thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments.
 
VESTAMID® E62-S3 is especially developed for sport shoe soles. It has good impact strength at low temperatures.

VESTAMID® E62-S3 is supplied as spherical pellets in moisture-proof packaging, ready for processing.
 
The process temperatures should be within a range of 190°C – 230°C.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 20 / * cm³/10min ISO 1133
Temperature 240 / * °C -
Load 2.16 / * kg -
Molding shrinkage, parallel 0.8 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.4 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 370 / 365 MPa ISO 527
Yield stress 23 / 24 MPa ISO 527
Yield strain 30 / 26 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 120 / 112 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 8 / 11 kJ/m² ISO 179/1eA
Type of failure C / C - -
Tensile notched impact strength, +23°C 230 / - kJ/m² ISO 8256/1
Stress at 10% elongation 19 / * MPa ISO 527
Stress at 100% elongation 23 / * MPa ISO 527
Stress at 300% elongation 40 / * MPa ISO 527
Strain at break TPE >300 / * % ISO 527
Compression set at 23 °C, 24h 34 / * % ISO 815
Compression set at 70 °C, 24h 48 / * % ISO 815
Compression set at 100 °C, 24h 85 / * % ISO 815
Shore D hardness 62 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 172 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 10 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 45 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 100 / * °C ISO 75-1/-2
Vicat softening temperature, B 110 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 200 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 200 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 9 / - - IEC 62631-2-1
Relative permittivity, 1MHz 4 / - - IEC 62631-2-1
Dissipation factor, 100Hz 1000 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 1200 / - E-4 IEC 62631-2-1
Volume resistivity 2E10 / 2.5E9 Ohm*m IEC 62631-3-1
Electric strength 39 / 35 kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 0.5 / * % Sim. to ISO 62
Density 1030 / - kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , VESTAMID® E62-S3, TPA, Evonik
Shearstress-shear rate , VESTAMID® E62-S3, TPA, Evonik
Stress-strain , VESTAMID® E62-S3 (dry), TPA, Evonik
Secant modulus-strain , VESTAMID® E62-S3 (dry), TPA, Evonik
Stress-Strain (TPE) , VESTAMID® E62-S3, TPA, Evonik
Stress-strain (isochronous) 23°C, VESTAMID® E62-S3 (cond.), TPA, Evonik
Creep modulus-time 23°C, VESTAMID® E62-S3 (cond.), TPA, Evonik
Creep curve 23°C, VESTAMID® E62-S3 (cond.), TPA, Evonik
Specific volume-temperature (pvT) , VESTAMID® E62-S3, TPA, Evonik
Tensile modulus-temperature , VESTAMID® E62-S3 (dry), TPA, Evonik
Characteristics
Processing
Injection Molding, Profile Extrusion, Other Extrusion
Delivery form
Pellets
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Applications
Sports Equipment
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com