Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9304 BK E70238 - PA612-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9304 BK E70238:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

High-viscosity, heat- and light-stabilized, impact-modified polyamide 612 compound for extrusion

VESTAMID® DX9304 BK E70238 is a PA 612 extrusion compound developed for the manufacturing of tubing systems with higher demands on heat resistance.
 

The melting point of VESTAMID® DX9304 BK E70238, about 35 °C higher than PA 11 and PA 12 compounds, allows higher temperatures in use. The compound is especially suitable for the extrusion of tubing systems that are exposed to high burst pressures at high service temperatures, e.g. hydraulic clutch lines.
 

The material absorbs only little moisture. Therefore dimensions and properties of parts are nearly unaffected through ambient conditions.

The process temperatures should be in the range of 240-270°C.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general recommendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 7 / * cm³/10min ISO 1133
Temperature 280 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 2.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.2 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1850 / 1200 MPa ISO 527
Yield stress 50 / 41 MPa ISO 527
Yield strain 5 / 20 % ISO 527
Nominal strain at break 41 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 40 / 95 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 30 / 18 kJ/m² ISO 179/1eA
Type of failure C / C - -
Shore D hardness 75 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 213 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 170 / * °C ISO 75-1/-2
Vicat softening temperature, B 175 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 150 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.1 / - - IEC 62631-2-1
Relative permittivity, 1MHz 3.2 / - - IEC 62631-2-1
Dissipation factor, 100Hz 560 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 310 / - E-4 IEC 62631-2-1
Volume resistivity 3.2E12 / 1.8E10 Ohm*m IEC 62631-3-1
Electric strength 39 / 38 kV/mm IEC 60243-1
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 2.7 / * % Sim. to ISO 62
Humidity absorption 1.3 / * % Sim. to ISO 62
Density 1040 / 1040 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Characteristics
Processing
Pipe/Tube Extrusion, Profile Extrusion
Delivery form
Pellets, Black
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.