Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L2140 BK 9.7504 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L2140 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

High viscosity, heat and light stabilized PA12 Compound

VESTAMID® L2140 BK 9.7504 is a heat- and light- stabilized polyamide 12 compound for the extrusion of tubing (e.g. fuel lines) and semi-finished products. Tubing according to DIN 73 378, Type: PA 12-HL.

Properties of compounds based on PA12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

The values presented are typical or average values, they do not constitute a specification.
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 6 / * cm³/10min ISO 1133
Temperature 230 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.6 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.3 / * % ISO 294-4, 2577
Density of melt 860 kg/m³ -
Thermal conductivity of melt 0.2 W/(m K) -
Spec. heat capacity of melt 3000 J/(kg K) -
Ejection temperature 170 °C -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1550 / 1300 MPa ISO 527
Yield stress 45 / 41 MPa ISO 527
Yield strain 4 / 13 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 16 / 12 kJ/m² ISO 179/1eA
Type of failure C / C - -
Charpy notched impact strength, -30°C 9 / 10 kJ/m² ISO 179/1eA
Type of failure C / C - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 176 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 40 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 110 / * °C ISO 75-1/-2
Vicat softening temperature, B 140 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 140 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 140 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Yellow Card available yes / * - -
Yellow Card available yes / * - -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.7 / 4.8 - IEC 62631-2-1
Relative permittivity, 1MHz 3 / 3.3 - IEC 62631-2-1
Dissipation factor, 100Hz 450 / 700 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 260 / 500 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 3E12 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E15 Ohm IEC 62631-3-2
Electric strength 26 / 36 kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.5 / * % Sim. to ISO 62
Humidity absorption 0.7 / * % Sim. to ISO 62
Density 1010 / 1010 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Characteristics
Processing
Injection Molding, Pipe/Tube Extrusion, Profile Extrusion, Other Extrusion
Delivery form
Pellets, Black
Additives
Lubricants
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Features
Tribologic Grade
Chemical Resistance
General Chemical Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.