Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9117 BK - PA12-(GF+CD) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9117 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Electrically polyamide 12 compound for quick connectors

VESTAMID® LX9117 BK 
is a glass-fiber-reinforced, electrically conductive PA12 molding compound that was developed in particular for the injection molding of connecting elements for fuel line systems (such as quick connectors).
 
The electrical conductivity of VESTAMID® LX9117 BK changes only slightly on contact with fuels, even if they contain alcohol. This is of great importance for use in fuel-conducting systems.
 
The material also has the advantageous properties characteristic of polyamide 12. The low water absorption leads to good dimensional stability of components in changing ambient humidity, and the other properties also remain virtually unchanged.
 
VESTAMID® LX9117 BK is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Our technical experts would appreciate to give you support regarding the special requirements for the processing of VESTAMID® LX9117 BK.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
 
The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.3 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 7930 / - MPa ISO 527
Yield stress 127 / - MPa ISO 527
Yield strain 4 / - % ISO 527
Nominal strain at break 4 / - % ISO 527
Charpy impact strength, +23°C 70 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Charpy impact strength, -30°C 50 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Charpy notched impact strength, +23°C 10 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Charpy notched impact strength, -30°C 9 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 177 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 40 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 169 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 179 / * °C ISO 75-1/-2
Vicat softening temperature, B 173 / * °C ISO 306
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 0.6 / * % Sim. to ISO 62
Density 1330 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding, Casting
Delivery form
Pellets, Black
Additives
Release agent
Special Characteristics
Increased electrical conductivity, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Applications
Electrical and Electronical
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com