Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7297 BK 9.7507 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7297 BK 9.7507:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
High viscosity, plasticized, impact-modified, heat- and light stabilized PA 12 compound

VESTAMID® X7297 BK 9.7507 is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of flexible tubing and hose especially for automotive applications.

 

VESTAMID® X7297 BK 9.7507 is characterized by easy processing as well as high impact strength at low temperatures.

 

Properties of compounds based on polyamide 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.
 

VESTAMID® X7297 BK 9.7507 is supplied as cylindrical pellets, ready for processing, in moisture-proof bags.

The use of colorants may affect property values. 
  
Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 13 / * cm³/10min ISO 1133
Temperature 230 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.9 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.3 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 390 / 390 MPa ISO 527
Yield stress 26 / 25 MPa ISO 527
Yield strain 37 / 37 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 122 / 130 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 6 / 8 kJ/m² ISO 179/1eA
Type of failure C / C - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 171 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 41 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 51 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 135 / * °C ISO 75-1/-2
Vicat softening temperature, B 125 / * °C ISO 306
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 11.4 / 13.7 - IEC 62631-2-1
Relative permittivity, 1MHz 3.6 / 3.8 - IEC 62631-2-1
Dissipation factor, 100Hz 1850 / 2260 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 1040 / 1570 E-4 IEC 62631-2-1
Volume resistivity 3.3E9 / 6.3E8 Ohm*m IEC 62631-3-1
Electric strength 36 / 36 kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Water absorption 1.4 / * % Sim. to ISO 62
Humidity absorption 0.8 / * % Sim. to ISO 62
Density 1020 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 220 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Characteristics
Processing
Pipe/Tube Extrusion, Other Extrusion
Delivery form
Pellets, Black
Additives
Plasticizer
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Features
Tribologic Grade
Chemical Resistance
General Chemical Resistance
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.