Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® HI19 - PBT-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® HI19:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Unreinforced polybutylene terephthalate compound with increased flexibility and toughness

VESTODUR® HI19 is an unreinforced, semicrystalline resin, based on polybutylene terephthalate with increased flexibility and toughness for the injection molding and extrusion process.

 

VESTODUR® HI19 is suitable for the manufacture of parts with high mechanical and thermal resistance. The product contains antioxidant agents and processing aids.

 

VESTODUR® HI19 is supplied as cylindrical pellets in polyethylene packaging.

 

For information about VESTODUR® HI19, please follow the general recommendations in our flyer "VESTODUR® Polybutylene terephthalate - Compounds”.

 

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

 

Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 12 / * cm³/10min ISO 1133
Temperature 250 / * °C -
Load 2.16 / * kg -
Molding shrinkage, parallel 1.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.4 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 460 / - MPa ISO 527
Yield stress 27 / - MPa ISO 527
Yield strain 23 / - % ISO 527
Nominal strain at break >50 / - % ISO 527
Tensile creep modulus, 1h * / 450 MPa ISO 899-1
Tensile creep modulus, 1000h * / 340 MPa ISO 899-1
Charpy impact strength, +23°C N / - kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 17 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Charpy notched impact strength, -30°C 8 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Tensile notched impact strength, +23°C 250 / - kJ/m² ISO 8256/1
Shore D hardness 65 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 197 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 2 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 110 / * °C ISO 75-1/-2
Vicat softening temperature, B 125 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 150 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 150 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4 / - - IEC 62631-2-1
Relative permittivity, 1MHz 3.6 / - - IEC 62631-2-1
Dissipation factor, 100Hz 220 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 330 / - E-4 IEC 62631-2-1
Volume resistivity >1E13 / - Ohm*m IEC 62631-3-1
Surface resistivity * / 1E14 Ohm IEC 62631-3-2
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 0.4 / * % Sim. to ISO 62
Humidity absorption 0.1 / * % Sim. to ISO 62
Density 1260 / - kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , VESTODUR® HI19, PBT-I, Evonik
Shearstress-shear rate , VESTODUR® HI19, PBT-I, Evonik
Stress-strain , VESTODUR® HI19 (dry), PBT-I, Evonik
Secant modulus-strain , VESTODUR® HI19 (dry), PBT-I, Evonik
Stress-strain (isochronous) 23°C, VESTODUR® HI19 (dry), PBT-I, Evonik
Creep modulus-time 23°C, VESTODUR® HI19 (dry), PBT-I, Evonik
Creep curve 23°C, VESTODUR® HI19 (dry), PBT-I, Evonik
Tensile modulus-temperature , VESTODUR® HI19 (dry), PBT-I, Evonik
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion, Coating
Delivery form
Pellets
Additives
Release agent
Special Characteristics
High impact or impact modified, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Features
Thermal Stability
Chemical Resistance
Oxidation Resistance
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.