Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VOLTALEF 302 - PCTFE - ARKEMA

Material Data Center offers the following functions for VOLTALEF 302:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Voltalef datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
VOLTALEF 302 resin is a fluorinated polymer which presents an exceptional behavior at very low temperatures.  It is usable in continuation from -200°C to 150°C with allowable peaks at 200°C. It is non-inflammability, has excellent chemical and radiation resistance, good barrier properties, is insensitivity to oxygen and water with good electrical properties.

The processing is critical but can be done by extrusion, injection and compression molding.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1400 MPa ISO 527
Yield stress 43 MPa ISO 527
Yield strain 7 % ISO 527
Nominal strain at break >50 % ISO 527
Charpy notched impact strength, +23°C 80 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 214 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 55 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 126 °C ISO 75-1/-2
Oxygen index 100 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 2E12 Ohm*m IEC 62631-3-1
Surface resistivity 1E15 Ohm IEC 62631-3-2
Electric strength 21 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.01 % Sim. to ISO 62
Humidity absorption 0.01 % Sim. to ISO 62
Density 2130 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding, Film Extrusion, Other Extrusion, Transfer Molding
Delivery form
Powder
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com