Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vu-Stat® Y-20 - PMMA - Röhm GmbH

Material Data Center offers the following functions for Vu-Stat® Y-20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vu-Stat datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Productprofil:

Vu-Stat Y-20 compound is a transparent, electro-static dissipative acrylic-based multipolymer mainly for molding medical applications.

Typical properties of of Vu-Stat Y-20 compound are:
• inherent and permanent static- dissipative properties, not surface treatment
• excellent bonding and welding capabilities
• good light transmission
• prevents drugs from adhering to application device
• high melt flow rate

Application:

Used for drug delivery devices, inhalation devices, electronic packaging and any application where anti-static protection is required.

Example:

Inhalers, needle hubs for bracheotherapy, radioactive seed implants and electronic components requiring dust resistant surfaces.

Processing:

Vu-Stat Y-20 compound can be processed with 3- zone general purpose screws for engineering thermoplastics.

Physical Form / Packaging:

Available in 1500 lb. gaylord boxes; other packaging available on request.

 

Regulatory and compliance requirements:

Meets requirements of the United States Pharmacopeia Class VI in 001 tint only; ISO 10993-1 in 001 tint only and FDA for food contact for all use conditions up to and including hot filled or pasteurized above 150  degrees F (e.g. Condition 21 CFR 176.170) for all food types except those containing more than 8% alcohol.

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4.8 cm³/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
Ejection temperature 71 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1500 MPa ISO 527
Yield stress 34.1 MPa ISO 527
Yield strain 4.4 % ISO 527
Charpy impact strength, +23°C 112 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6.8 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 89 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 96 °C ISO 75-1/-2
Vicat softening temperature, B 91 °C ISO 306
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 84 % ISO 13468-1, -2
Other propertiesValueUnitTest Standard
Density 1120 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 3 - 4 h -
Melt temperature 200 - 250 °C -
Mold temperature 30 - 60 °C -
Diagrams
Stress-strain , Vu-Stat® Y-20, PMMA, Röhm
Secant modulus-strain , Vu-Stat® Y-20, PMMA, Röhm
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Anti-static, Transparent
Features
Good Adhesion, Weldable
Certifications
Food contact, Food approval FDA 21 CFR, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Electrical and Electronical, Medical, Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Predrying temperature: 80 °C
Predrying time: 3 - 4 h
PROCESSING
Melt temperature: 200 - 250°C
Mold temperature:30 - 60°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com