Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 66A NT0766 - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 66A NT0766:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Vydyne 66A NT0766 is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. 66A NT0766 resin offers high strength, rigidity and toughness over a broad range of demanding applications and good fluid resistance to a wide variety of chemicals, solvents and oils.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 2.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 2.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2800 / 1800 MPa ISO 527
Yield stress 85 / 55 MPa ISO 527
Yield strain 5 / 20 % ISO 527
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6 / 23 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 6 / 6 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 70 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 195 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 100 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 100 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Oxygen index 28 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Electric strength 26 / - kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Humidity absorption 2.5 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Sheet Extrusion
Delivery form
Pellets, Natural Color
Chemical Resistance
General Chemical Resistance, Solvent Resistance, Oil Resistance
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com