Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R220 - PA66-MX40 - Ascend

Material Data Center offers the following functions for Vydyne® R220:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Vydyne R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing advantages of unreinforced PA66 while enhancing rigidity, strength and heat resistance. R220 maintains the chemical resistance typical of PA66 to a wide variety of chemicals, gasoline, oils, greases and solvents.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 1.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 6900 / 2600 MPa ISO 527
Yield stress 103 / 73 MPa ISO 527
Yield strain 1.5 / 16 % ISO 527
Charpy impact strength, +23°C 140 / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 110 / 130 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 7 / 17 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 6 / 8 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 258 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 118 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 222 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 63 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 60 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 1.6 / * % Sim. to ISO 62
Density 1480 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Natural Color
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Features
Ductile
Chemical Resistance
General Chemical Resistance, Solvent Resistance, Grease Resistance, Oil Resistance
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.