Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R433H BK0746 - PA66-GF33 - Ascend

Material Data Center offers the following functions for Vydyne® R433H BK0746:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Vydyne R433H BK0746 is designed to reinforce downgauged steel and aluminum used in vehicle body-in-white (BIW) structures, helping reduce weight without sacrificing safety or comfort.
R433H BK0746 has improved energy absorption over traditional glass-filled PA66, helping reduce noise, vibration and harshness (NVH) and absorbing impact energy from crashes. Using R433H BK0746 in the BIW structure reinforces sheet metal, helping manufacturers shave substantial weight and improve efficiency. Trends in lightweight and NVH are becoming even more paramount with the growth of Electric Vehicles. Vydyne R433H BK0746 has excellent performance attributes to support applications where this will be of prime importance such as battery frames and housings.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.6 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 9600 / 6200 MPa ISO 527
Yield stress 150 / 103 MPa ISO 527
Yield strain 3.3 / 7.4 % ISO 527
Flexural modulus, 23°C 8400 / 6000 MPa ISO 178
Flexural strength 210 / 130 MPa ISO 178
Charpy impact strength, +23°C 96 / 96 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 100 / 92 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 24 / 27 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 17 / 16 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 21 / 29 kJ/m² ISO 180/1A
Izod notched impact strength 15 / - kJ/m² ISO 180/1A
Temperature -40 °C -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 262 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 245 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 260 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 16 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 11 / * E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Burning Behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 0.4 / * mm -
ASTM Data
UL 94 Flame rating V-2 - UL 94
Thickness tested 0.4 mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Electric strength 28 / - kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Water absorption 1 / * % Sim. to ISO 62
Humidity absorption 1.3 / * % Sim. to ISO 62
Density 1350 / - kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
Melt temperature 285 - 305 °C -
Mold temperature 65 - 95 °C -
Zone 1 280 - 310 °C -
Zone 2 280 - 310 °C -
Zone 3 280 - 310 °C -
Nozzle temperature 280 - 310 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Additives
Lubricants
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Features
Acoustical Barrier Properties
Chemical Resistance
General Chemical Resistance, Solvent Resistance, Oil Resistance
Applications
Automotive, Encapsulation
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.