Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R535H BK0783 - PA66-GF35 - Ascend

Material Data Center offers the following functions for Vydyne® R535H BK0783:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Vydyne R535H BK0783 is a general purpose, 35% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. R535H BK0783 offers improved flow with a black surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.9 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 11600 / 8500 MPa ISO 527
Stress at break 210 / 150 MPa ISO 527
Strain at break 3 / 5 % ISO 527
Charpy impact strength, +23°C 80 / 90 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 70 / 85 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 12 / 14 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 11 / 12 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 250 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 260 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 20 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 105 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E11 / - Ohm*m IEC 62631-3-1
Electric strength 20 / - kV/mm IEC 60243-1
Comparative tracking index 325 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 0.8 / * % Sim. to ISO 62
Humidity absorption 1.6 / * % Sim. to ISO 62
Density 1410 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Black
Additives
Lubricants
Special Characteristics
Heat stabilized or stable to heat
Chemical Resistance
General Chemical Resistance, Solvent Resistance, Oil Resistance
Applications
General Purpose
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.