Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of WONDERLOY PC-385 - (PC+ABS) - Chi Mei Corporation

Material Data Center offers the following functions for WONDERLOY PC-385:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Wonderloy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 21 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
Molding shrinkage, parallel 0.5 % ISO 294-4, 2577
ASTM Data
Melt Flow Index, MFI 21 g/10min ASTM D 1238
Temperature 260 °C -
Load 5 kg -
Mold Shrinkage, MD 0.005 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 55 MPa ISO 527
Stress at break 57 MPa ISO 527
Flexural modulus, 23°C 2300 MPa ISO 178
Flexural strength 85 MPa ISO 178
Charpy notched impact strength, +23°C 55 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 45 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 55 kJ/m² ISO 180/1A
Izod notched impact strength 45 kJ/m² ISO 180/1A
Temperature -30 °C -
ASTM Data
Tensile Strength at Yield 53 MPa ASTM D 638
Elongation at Break 90 % ASTM D 638
Flexural Modulus 2305 MPa ASTM D 790
Flexural Strength 78.5 MPa ASTM D 790
Rockwell Hardness R 114 - ASTM D 785
Izod Impact notched, 1/8 in 587 J/m ASTM D 256
Izod Impact notched, Low-Temperature 491 J/m ASTM D 256
Temperature -34.4 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 108 °C ISO 75-1/-2
Vicat softening temperature, A 143 °C ISO 306
Vicat softening temperature, B 135 °C ISO 306
Coeff. of linear therm. expansion, parallel 75 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 1.5 mm -
Coefficient of Thermal Expansion, MD 135 E-6/K ASTM D 696
DTUL @ 264 psi 110 °C ASTM D 648
Vicat Temperature 140 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Volume resistivity 1E16 Ohm*m IEC 62631-3-1
Surface resistivity 1E16 Ohm IEC 62631-3-2
ASTM Data
Dielectric Constant, 1 MHz 3 - ASTM D 150
Surface Resistivity 1E16 Ohm ASTM D 257
Volume Resistivity 1E14 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Density 1150 kg/m³ ISO 1183
Density 1150 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 100 °C -
Pre-drying - Time 4 h -
Mold temperature 50 - 100 °C -
Feed temperature 200 - 230 °C -
Zone 1 230 - 270 °C -
Nozzle temperature 220 - 260 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Applications
Automotive, Electrical and Electronical, General Purpose
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.