Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of WONDERLOY PC-545 - (PC+ABS) - Chi Mei Corporation

Material Data Center offers the following functions for WONDERLOY PC-545:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Wonderloy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 10 cm³/10min ISO 1133
Temperature 260 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.2 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 63 MPa ISO 527
Stress at break 62 MPa ISO 527
Flexural modulus, 23°C 2400 MPa ISO 178
Flexural strength 94 MPa ISO 178
Charpy notched impact strength, +23°C 60 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 14 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 63 kJ/m² ISO 180/1A
Izod notched impact strength 15 kJ/m² ISO 180/1A
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 102 °C ISO 75-1/-2
Vicat softening temperature, A 127 °C ISO 306
Vicat softening temperature, B 121 °C ISO 306
Coeff. of linear therm. expansion, parallel 80 E-6/K ISO 11359-1/-2
Burning behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 1.2 mm -
Yellow Card available yes - -
Burning behav. 5V at thickness h 5VA class IEC 60695-11-20
Thickness tested 2.5 mm -
Yellow Card available yes - -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.1 - IEC 62631-2-1
Volume resistivity 3.9E15 Ohm*m IEC 62631-3-1
Surface resistivity 2.9E15 Ohm IEC 62631-3-2
ASTM Data
Dielectric Strength, Short Time 1.22 kV/mm ASTM D 149
Arc Resistance 150 s ASTM D 495
Other propertiesValueUnitTest Standard
Density 1190 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 90 °C -
Pre-drying - Time 4 h -
Mold temperature 40 - 70 °C -
Feed temperature 210 - 230 °C -
Zone 1 240 - 260 °C -
Nozzle temperature 230 - 250 °C -
Characteristics
Processing
Injection Molding
Additives
Flame retarding agent
Special Characteristics
Flame retardant, Heat stabilized or stable to heat
Applications
IT / Business Machine, Electrical and Electronical
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.