Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Zylar® 550 - MBS-I - INEOS Styrolution

Material Data Center offers the following functions for Zylar® 550:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Zylar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Zylar® 550 is an impact modified styrene acrylic copolymer that provides practical toughness, good clarity and superior processing characteristics for demanding injection molded applications.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 55 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2100 MPa ISO 527
Yield stress 28 MPa ISO 527
Yield strain 2 % ISO 527
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 4 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 81 °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1.5 % ASTM D 1003
Light Transmittance 90 % ASTM D 1003
Other propertiesValueUnitTest Standard
Water absorption 0.1 % Sim. to ISO 62
Humidity absorption 0.05 % Sim. to ISO 62
Density 1050 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 210 °C ISO 294
Injection Molding, mold temperature 50 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
High impact or impact modified, Transparent, Sterilizable, Ethylene Oxide (EtO) Sterilization, Gamma irradiation sterilization
Features
Copolymer
Chemical Resistance
Radiation Resistance
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved, Drug Master File, Long term supply assurance
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Pre-drying, Temperature: 65 °C
Pre-drying, Time: 2 h

PROCESSING
injection molding, Melt temperature, range: 200 - 240 °C
injection molding, Melt temperature, recommended: 210 °C
injection molding, Mold temperature, range: 30 - 55 °C
injection molding, Mold temperature, recommended: 50 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.