Hydrochloric Acid (36% by mass) (23°C)

A meaningful evaluation of the resistance of any resin
against chemical reagents has to take the end-use
conditions into consideration.

The ratings listed here are based on our long-term
experience with the field performance of parts as well
as extensive lab testing.

For more Info please refer to the
linked dokuments or call our representatives.


Disclaimer Chemical Resistance
The chemical resistance data reported here are based on either measured weight/dimensional changes or degree of chemical attack determined from exposure in accordance with one of the relevant established international standards (ISO 175, ISO 11403-3, ISO 4599, ISO 4600, ISO 6252 etc.) or on the supplier´s experiences from successful applications of their products. Due to the application specific nature of the surrounding environment of each part during its service life, the indications provided should be used only for a first assessment; they are not intended to substitute for any testing you may need to conduct. You must make your own determination as to the suitibility of this material for your specific application. Users shall in each case conduct evaluations under actual end-use conditions and/or consult with the resin supplier´s technical representatives.