Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of AVALON® 80 ABX - TPU - Huntsman Polymers Corp.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Avalon datasheets, application examples or technical articles are available in Material Data Center
Mechanical properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Other Standards[S] | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Tensile Strength | 25 | MPa | DIN 53504 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Strain at break | 650 | % | DIN 53504 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Tear strength | 35 | kN/m | DIN 53507 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Abrasion resistance | 55 | mm³ | DIN 53516 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Shore A hardness | 81 | - | DIN 53505 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Shore D hardness | 30 | - | DIN 53505 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Other Standards[S] | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Density | 1150 | kg/m³ | DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature | 80 - 90 | °C | - |
Pre-drying - Time | 2 | h | - |
Mold temperature | 25 - 50 | °C | - |
Feed temperature | 25 - 35 | °C | - |
Zone 1 | 170 - 190 | °C | - |
Zone 2 | 175 - 195 | °C | - |
Zone 3 | 175 - 200 | °C | - |
Nozzle temperature | 170 - 195 | °C | - |
Screw speed | 20 - 80 | rpm | - |
Injection pressure | 2 - 10 | MPa | - |
Back pressure | 0.03 - 0.3 | MPa | - |
Holding pressure | 1 - 5 | MPa | - |