Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bakelite® UP 3720 - UP-X - Bakelite Synthetics

Material Data Center offers the following functions for Bakelite® UP 3720:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bakelite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Product description:

Polyester moulding compound, mainly organically filled, styrene free, very slight post shrinkage, very good electrical properties, very good sliding friction properties, dimensionally stable, UL listed moulding compound 0,8 mm / V1 (ALL), 1,5 mm / V-0 (ALL).

Application areas:

Bearings, guide rails, cross bars, micro switches, regulator switch cylinders.

Property Name Value Unit Standard No.
Apparent density (moulding compound) 0.64 g/cm³ ISO 60
Moulding shrinkage (injection moulding, longitudinal)  0.75 % ISO 2577
Post shrinkage (injection moulding, 168h/110°C) 0.15 % ISO 2577
Moulding shrinkage (compression moulding, longitudinal)  0.35 % ISO 2577
Post shrinkage (compression moulding, 168h/110°C) 0.1 % ISO 2577
Tensile strength (5mm/min) 45 MPa ISO 527-1/2
Compr. strength (test spec. flat tested) 150 MPa ISO 604
Flexural strength (2mm/min) 90 MPa ISO 178
Flexural modulus 8000 MPa ISO 178
Ball indentation hardness (H 961/30) 250 MPa ISO 2039/P1
Water absorption (24h/23°C) 50
mg similar to ISO 62
Additional characteristics: low shrinkage/good dimensional stability, high arc resistance

Preparation of Test Specimens of Thermosetting Moulding Compound

  • Compression to ISO 295
  • Injection to ISO 10724


Storage capability
12 month (shorter shelf life for darker colours), (relative humidity of 50-60% and maximum storage temperature of approximately 20°C)

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.8 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 9000 MPa ISO 527
Charpy impact strength, +23°C 9 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 2.2 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 8.00 MPa 70 °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h V-1 class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 5 - IEC 62631-2-1
Dissipation factor, 100Hz 0.03 E-4 IEC 62631-2-1
Volume resistivity 1E10 Ohm*m IEC 62631-3-1
Surface resistivity 1E11 Ohm IEC 62631-3-2
Electric strength 32.5 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1740 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, injection temperature 105 °C ISO 10724
Injection Molding, injection velocity 170 mm/s ISO 10724
Injection Molding, hold pressure 100 MPa ISO 10724
Injection Molding, cure time 25 min ISO 10724
Compression Molding, mold temperature 160 °C ISO 295
Compression Molding, cure time 1 min ISO 295
Diagrams
Dynamic Shear modulus-temperature , Bakelite® UP 3720, UP-X, Bakelite Synthetics
Stress-strain , Bakelite® UP 3720, UP-X, Bakelite Synthetics
Secant modulus-strain , Bakelite® UP 3720, UP-X, Bakelite Synthetics
Characteristics
Processing
Injection Molding, Transfer Molding
Regional Availability
Other text information
Injection molding
VERARBEITUNG
Temperature of material: 70 - 100 °C
Mould temperature: 160 - 180 °C
Curing time: 10-20 sec
 
Further Information:
Barrel temperature
  - Feed zone: 60-70 °C
  - Nozzle zone: 70-100 °C
Cavity moulding pressure: >10 MPa
Back pressure: 0.5-1 MPa
Holding pressure: 60% of injection pressure
Compression molding
PROCESSING
Mould temperature:160-180°C
Curing time:20-40sec
Cavity moulding pressure: >10MPa
Application examples
Power switches (insulator)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.