Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bio-Flex® FX 1821 - PLA... - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Bio-Flex® FX 1821:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Bio-Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Biodegradable and home compostable polymer compound. Certified as home compostable according to EN 13432 (at ambient temperature) with a maximum thickness of 32 μm. Suitable for blown film applications.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 3 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Melt flow index, MFI 3.7 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 155 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
Density 1380 kg/m³ ISO 1183
Film PropertiesValueUnitTest Standard
ISO Data
Tensile Modulus, parallel 150 MPa ISO 527-3
Tensile Modulus, normal 110 MPa ISO 527-3
Strain at yield, parallel 500 % ISO 527-3
Strain at yield, normal 570 % ISO 527-3
Stress at break, parallel 23 MPa ISO 527-3
Stress at break, normal 21 MPa ISO 527-3
Maximum strain, parallel 500 % ISO 527-3
Maximum strain, normal 570 % ISO 527-3
Type of extrusion blown - -
Thickness of specimen 0.03 mm -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion blown - -
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 190 °C -
Feed temperature 60 °C -
Zone 1 160 °C -
Zone 2 165 °C -
Zone 3 170 °C -
Zone 4 175 °C -
Nozzle temperature 180 °C -
Characteristics
Processing
Blown Film Extrusion, Film Extrusion
Delivery form
Pellets, White
Special Characteristics
Opaque
Certifications
Contains renewable resources, Biodegradable, Food contact, Compostable ISO 13432 (Producer), Compostable ISO 13432 (Certificate)
Applications
Packaging, Toys
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.