Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DOWLEX™ 2355 - PE - The Dow Chemical Company

Material Data Center offers the following functions for DOWLEX™ 2355:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Dowlex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 0.7 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 399 MPa ISO 527
Yield stress 14 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 36 MPa ISO 527
Strain at break 800 % ISO 527
Flexural modulus, 23°C 429 MPa ISO 178
Shore D hardness 59 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Coeff. of linear therm. expansion, parallel 270 E-6/K ISO 11359-1/-2
ASTM Data
Vicat Temperature 119 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 931 kg/m³ ASTM D 792
Characteristics
Processing
Other Extrusion
Features
Copolymer, Octene Copolymer
Chemical Resistance
Environmental Stress Crack Resistance
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Drinking water contact
Applications
Building Construction
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.