Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN067-30 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN067-30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastar™ Renew copolyester EN067-30 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability haracteristics. Due to slower crystallization kinetics, this product is capable of producing a part free of crystalline haze upon injection molding. This product is tailored for the injection-molded cosmetics and personal care market.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.


Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.0035 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 57 MPa ASTM D 638
Tensile Strength at Break 24 MPa ASTM D 638
Elongation at Yield 4 % ASTM D 638
Elongation at Break 134 % ASTM D 638
Flexural Modulus 2600 MPa ASTM D 790
Flexural Strength 81 MPa ASTM D 790
Rockwell Hardness 110 - ASTM D 785
Izod Impact notched, 1/8 in 58 J/m ASTM D 256
Izod Impact notched, Low-Temperature 29 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 66 °C ASTM D 648
DTUL @ 264 psi 61 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Light Transmittance 84 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1320 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 150 - 160 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 270 - 290 °C -
Mold temperature 10 - 30 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Features
Copolymer
Certifications
ISCC Plus
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com