Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EB062 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EB062:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastar™ EB062 copolyester is a resin specifically designed for extrusion blow-molded bottles and jars for use in food and beverage and home care applications. Its high drop strength makes it particularly well suited for containers that hold heavier contents, including liquids and dense solids. Eastar EB062 is recognized throughout

the industry for its best-in-class aesthetics and process ease. It has high-gloss clarity and is free of gels and unmelts that are common in some competitive resins. Eastar EB062 is a hassle-free, economical choice for replacing materials of concern, such as polyvinyl chloride (PVC), in consumer packaging. This product is certified

to NSF/ANSI Standard 51 for Food Equipment Materials.






Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.003 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1900 MPa ASTM D 638
Tensile Strength at Yield 47 MPa ASTM D 638
Tensile Strength at Break 48 MPa ASTM D 638
Elongation at Yield 5 % ASTM D 638
Elongation at Break 300 % ASTM D 638
Flexural Modulus 1900 MPa ASTM D 790
Flexural Strength 65 MPa ASTM D 790
Rockwell Hardness 105 - ASTM D 785
Izod Impact notched, 1/8 in N J/m ASTM D 256
Izod Impact notched, Low-Temperature 63 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 73 °C ASTM D 648
DTUL @ 264 psi 63 °C ASTM D 648
Vicat Temperature 85 °C ASTM D 1525
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 143 - ASTM D 2457
Haze 1.3 % ASTM D 1003
Light Transmittance 91 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1250 kg/m³ ASTM D 792
Characteristics
Processing
Blow Molding
Special Characteristics
Transparent
Features
Barrier Properties, High Gloss, Copolymer
Certifications
Food contact, Food approval NSF 51, Food contact notification (FCN)
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.