Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN076 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN076:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastar™ EN076 copolyester is a clear copolyester used in a variety of packaging and consumer product applications, including food and beverage packaging, general purpose packaging, flexible film packaging, and consumer products. It is fully compatible with the resin identification code 1 (RIC1) recycle stream. Eastar EN076

enables fast-moving consumer-goods brand owners to achieve recyclable products and packaging and replace materials of concern without sacrificing aesthetics.


Eastar EN076 meets the definition of resin identification code PREPROCESSING (RIC1) as defined by ASTM D7611. Other endproduct attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability.


Eastar EN076 copolyester may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.




Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.0035 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 56 MPa ASTM D 638
Tensile Strength at Break 26 MPa ASTM D 638
Elongation at Yield 4 % ASTM D 638
Elongation at Break 75 % ASTM D 638
Flexural Modulus 2350 MPa ASTM D 790
Rockwell Hardness 111 - ASTM D 785
Izod Impact notched, 1/8 in 67 J/m ASTM D 256
Izod Impact notched, Low-Temperature 33 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 69 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 0.8 % ASTM D 1003
Light Transmittance 89 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1320 kg/m³ ASTM D 792
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 150 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 277 - 293 °C -
Mold temperature 16 - 32 °C -
Characteristics
Processing
Injection Molding, Film Extrusion, Other Extrusion, Thermoforming
Features
Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com