Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ MN005 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ MN005:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastar™ Copolyester MN005 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and EtO sterilization. Eastar™ Copolyester MN005 has excellent appearance and is nearly waterclear.


It is easy to process and can fill intricate tools. Its most outstanding features are exceptional clarity, toughness, radiation resistance chemical resistance and excellent color and property retention following gamma and e-beam sterilization. MN005 contains a mold release.




Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.003 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 47 MPa ASTM D 638
Tensile Strength at Break 38 MPa ASTM D 638
Elongation at Yield 5 % ASTM D 638
Elongation at Break 260 % ASTM D 638
Flexural Modulus 1900 MPa ASTM D 790
Rockwell Hardness 104 - ASTM D 785
Izod Impact notched, 1/8 in N J/m ASTM D 256
Izod Impact notched, Low-Temperature 69 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 70 °C ASTM D 648
DTUL @ 264 psi 67 °C ASTM D 648
Vicat Temperature 84 °C ASTM D 1525
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 90 % ASTM D 1003
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.15 % ASTM D 570
Density 1230 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 75 °C -
Pre-drying - Time 6 h -
Melt temperature 250 - 270 °C -
Mold temperature 15 - 30 °C -
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
Transparent, Sterilizable, Ethylene Oxide (EtO) Sterilization, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Features
Color Stability, Copolymer
Chemical Resistance
General Chemical Resistance, Solvent Resistance, Radiation Resistance
Certifications
Food contact, Food approval FDA 21 CFR, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.